Barium titanate BaTiO3-based thick film capasitors have been fabricated by adding 5% of frit which sinterred at 700-900ºC. Barium titanate powder were synthesized by using barium carbonate (BaCO3) powder and titanium oxide (TiO2) in molar ratio 50% : 50%. The obtained powder were shaped as pellets and calcined at temperature of 1100ºC for 2 hours. After that, BaTiO3 powder homogened and combi…